Film thickness and coating rate
Minimum Maximum Typical
Dry film thickness (um) 30 80 50
Wet film thickness (um) 45 120 80
Theoretical coating rate (m2/kg) 10 5 8
Physical character
Color Silver gray
Solid contents 70
flashing point nil
Gloss Semi-gloss
Water-resistance Favorable
Flexibility excellent
Surface Treatment
All surfaces should be clean, dry and free from dirt, and the surface should follow
ISO8504 before evaluation and processing.
Steel coated with primer
clean, dry, and approved primer
Steel coated with waterborne epoxy zinc-rich primer or waterborne inorganic zinc-rich
primer
Clean and dry primer. Sand blast is needed if primer overseeds the maximum re-coating
XGE-HY-B(A , B )
Water-based epoxy barrior paint
2 / 5
interval.
Other surfaces
This product can be applied on other substrate. Refer the details to the company.
Engineering Method
Substrate temperature must not be lower than 10°and should be at least 6°or more above
the dew point of the air temperature and relative humidity should be measured near the
substrate. In narrow area
Good ventilation is usually required to ensure proper drying.
Manner of application
Spray coat Use airless spray or air spray.
Brush coat It is recommended for pre-coating and small-area coating, but the required
dry film thickness must be achieved.
Roll coat It can be used in small areas, but it is not recommended as the first primer.
In the case of roller coating, sufficient materials must be applied to
achieve the specified dry film thickness.